ITER Fusion Reactor Delays as Chlorine Corrosion Forces Three-Year Thermal Shield Overhaul
energy2 months ago

ITER Fusion Reactor Delays as Chlorine Corrosion Forces Three-Year Thermal Shield Overhaul

The ITER fusion project in southern France completed a three-year repair of its vacuum vessel thermal shield after chlorine trapped during cleaning caused stress corrosion cracks in cooling pipes. Workers removed 2,205 pounds of silver plating and cut 6.8 miles of piping to replace damaged sections. The fix, finished in July 2026, was completed ahead of schedule by contractor INOX-CVA, though the incident highlights how minor chemical residues can cause major delays in complex fusion hardware.